Coil

Filter dimensions for Coil

Coil
thickness (mm) - t
min. width (mm) - B
min. length (mm) - L

Results

Add this search to my alerts

1 Products

What does
Information provided by the seller.
and
Put to your attention, that the material is not imported into the EU. In order to avoid excessive custom taxes or administration, we advise you to contact us by using  (please click on the concerned position) in order to check the origin of the material.
stand for?
  Material Number - alloy thickness
(mm) - t
min. width
(mm) - B
Location Origin Surface Type Total
Quantity
(kg)
Min deliverable
quantity (kg) - lot
Price ▲    
3.7025 - Grade 1 2.00 917.00 CH, 8600 JP unknown, see information 980.00 980.00 €46.43 / kg Negotiate

Warning: Origin out of EU / not yet imported in the EU

1 lot(s)
Add to Cart

Ti Gr 1 / 3.7025

Unalloyed titanium offering optimum ductility and cold formability with useful strength, high-impact toughness and excellent weldability. This makes this grade suitable for the manufacture of components in weight-saving structures with reduced mass forces and also for components requiring high corrosion resistance. In addition, thermal stresses in titanium structures are lower than in other metallic materials, due to the low thermal expansion of titanium.

Material Data Sheet

Material designation 3.7025
EN Material Symbol Titan Grade 1
ASTM Ti-Grade 1
UNS R50250

Main fields of application of Titanium Gr 1

For corrosion resistance in the chemical and marine industries; in airframe construction where ease of formability is desired also widely used in the medical sector because of their outstanding biocompatibility.

Chemical composition of Titanium Gr 1

Ti Fe C O H N
% % % % % %
rest 0.2 0.08 0.18 0.015 0.03

Characteristics of Titanium Gr 1

Hardness HB 30 ≤ 30 120
0.2 % Yield strenght Rp ≥ N/mm² 170
Tensile strenght Rm N/mm² ≥ 240
Elongation ≥% 24
Modulus of elasticity kN/mm² 105

Filler metal (for welding with titanium Gr 1

Grade 1 has very good weldability. Being substantially single-phase material, the microstructure of the alpha phase is not affected greatly by thermal treatments or welding temperatures. Therefore, the mechanical properties of a correctly welded joint are equal to, or exceed those of the parent metal and show good ductility

Send an enquiry